1bwana1 wrote:
I am still not fully happy with my film workflow. I think I am getting too much grain in many of my images. Not sure if this is the result of poor digital processing, or happening in the film development stage. Does the chemistry used have an important impact on grain. I have been using a two part MonoBath Chemistry produced locally by ARS-Amago who made made Lab-Box, on Ilford HP5+-400.
Never mucked with monobath with traditional B+W. Even with the traditional 3-step process--Develop-Stop-Fix--only two chemicals are required, developer and non-hardening fixer. Water is fine for the stop.
If you want to go back to basic, tried and true, then start with either D-76 (Kodak) or ID-11 (Ilford). I'm a fan of Xtol for full speed, and finest grain. However, while an excellent emulsion, HP5+ is not noted for its fine grain.